stainless steel welding wire
We specialize in stainless steel wire, tiny wire, hydrogen-lost wire, smooth wire, etc.
Type
%Chemical Composition%
Mechanical properties
KSJIS)
ZPSS
C
Cr
Ni
Mo
Others
Heat Treatment
N/mm2 Yield strength
Tensile strength
% Elongation
Hardness
HB
HRB
HV
AUSTENITE
301
301
≤0.15
16.018.0
6.008.00
-
-
S
≥205
≥520
≥40
≤207
≤95
≤218
301L
301L
≤0.030
16.018.0
6.008.00
-
N≤0.20
S
≥215
≥550
≥45
≤187
≤90
≤200
304
304
≤0.08
18.020.0
8.0010.50
-
-
S
≥205
≥520
≥40
≤187
≤90
≤200
304J1
304Cu
0.020.05
16.517.1
7.57.9
-
Cu1.92.2
S
≥155
≥450
≥40
≤187
≤90
≤200
304L
304L
≤0.030
18.020.0
9.0013.00
-
-
S
≥175
≥480
≥40
≤187
≤90
≤200
304N1
304N1
≤0.08
18.020.0
7.0010.50
-
N0.100.25
S
≥275
≥550
≥35
≤217
≤95
≤220
304N2
304N2
≤0.08
18.020.0
7.5010.50
-
Nb≤0.15
S
≥345
≥690
≥35
≤248
≤100
≤260
309S
309S
≤0.08
S
≥175
≥520
≥40
≤187
≤90
≤200
316
316
≤0.08
16.018.0
10.0014.00
2.003.00
s
≥205
≥520
≥40
≤187
≤90
≤200
316L
316L
≤0.03
12.0015.00
S
≥175
≥480
≥40
≤187
≤90
≤200
321
321
≤0.08
17.019.0
9.0013.00
-
Ti5×C%over
S
≥205
≥520
≥40
≤187
≤90
≤200
FERRITE
409L
409L
≤0.03
17.019.0
-
-
Ti6×C%0.75
A
≥175
≥360
≥25
≤162
≤80
≤175
410L
410L
≤0.03
11.013.5
-
-
-
A
≥195
≥360
≥22
≤183
≤88
≤200
430LX
430LX
≤0.03
16.019.0
-
-
TiorNb0.11.0
A
≥175
≥360
≥22
≤183
≤88
≤200
430
430
≤0.12
16.018.0
A
≥205
≥450
≥22
≤183
≤88
≤200
430Ti
430Ti
≤0.03
19.021.0
TIO.20.5
A
≥205
≥420
≥25
≤162
≤80
≤175
430J1L
30J1L
≤0.025
16.020.0
-
-
Nb8(C%+N%)0.8Cu0.300.80
A
≥205
≥390
≥22
≤192
≤90
≤200
436L
436L
≤0.025
16.019.0
-
0.751.25
TiNbZr8×(C%+N%)0.8
A
≥245
≥410
≥20
≤217
≤96
≤230
444
444
≤0.025
17.020.0
1.752.50
Ti,Nb,Zr8×C%+N%)0.8
A
≥245
≥410
≥20
≤217
≤96
≤230
MARTENSITE
410
410
≤0.15
11.513.5
-
-
-
A
≥205
≥440
≥20
≤201
≤93
≤210
420J1
420J1
0.160.25
12.014.0
-
-
-
A
≥225
≥520
≥18
≤223
≤97
≤234
No comments: